MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Strator® A-3 HI N7 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: This product has been rebranded. The new name is Xencor™ PA66 LGF-1030 HI.

Strator® A-3 HI N7 is a high impact, 30% long glass fiber reinforced, easy-flowing PA66 with a pellet length of 7 mm which can be processed on most injection molding machines.

This material achieves extremely high mechanical and thermal properties, in combination with ease of processing and fast cycle times. It exhibits high strength, stiffness and impact strength at high temperatures; excellent creep and fatigue resistance; isotropic mechanical properties and reduced isotropic shrinkage; high shear strength and high burst pressure; and an excellent surface finish.

Applications: Aircraft Applications; Automotive Applications; Automotive Instrument Panel; Gears

Features: Creep Resistant; Electrically Insulating; Fatigue Resistant; High Impact Resistance; High Rigidity; High Stiffness; High Tensile Strength; Hot Water Moldability; Low CLTE; Low Warpage

Injection notes: Pre-Drying
Since polyamides are hygroscopic materials as well as sensitive to moisture during processing, this product should always be pre-dried. At a humidity content above 0.1%, the material will begin to degrade. Recommended drying time is 4 hours at 110°C in dry-air dryer.
Processing temperatures
Melt temperature should be kept below 310°C in order to prevent degradation. The exact setting depends from machine and mold design, but is usually within the following range:
Area | Recommendation:
Zone 1 (feed) 270-300°C | 280°C
Zone 2 270-300°C | 290°C
Zone 3 285-310°C | 295°C
Zone 4 (Nozzle) 285-320°C | 300°C
Mold temperature
The mold temperature is a compromise between the optimum properties that can be obtained from high crystallization, and cycle time. Strator® A-3 HI N7 can be processed at mold temperatures between 80°C and 160°C. Optimum surface quality requires a mold temperature above 100°C.
Regrind
Regrind of highly filled thermoplastic materials, such as Strator® A-3 HI N7, should only be recycled with special care. The regrind content must never exceed 15% and only regrind of optimum quality should be used. In any case, part properties should be checked.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccISO 1183
Moisture Absorption 1.70 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPaISO 527-2
Elongation at Break 2.9 %ISO 527-2
Tensile Modulus 10000 MPaISO 527-2
Flexural Strength 230 MPaISO 178
Flexural Modulus 9500 MPaISO 178
Charpy Impact Unnotched 100 kJ/m²ISO 179
Charpy Impact, Notched 45.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+12 ohmASTM D257
Dielectric Strength 35.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 255 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 250 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 270 - 300 °C
Middle Barrel Temperature 270 - 300 °C
Front Barrel Temperature 285 - 310 °C
Nozzle Temperature 285 - 320 °C
Melt Temperature <= 310 °CInjection
Mold Temperature 80.0 - 160 °C
Drying Temperature 110 °C
@Time 14400 sec
Moisture Content <= 0.10 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4495 / 280295

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.