MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Poco Graphite Premium Graphite EDM Graphite EDM-2® Graphite
Categories: Carbon; Graphite

Material Notes: EDM-2® graphite is an Ultrafine grade that displays high strength and good wear characteristics. EDM-2® graphite is an Ultrafine graphite with high strength and good wear characteristics. Recommended for use on detailed electrodes where speed, fine finish, and resistance to wear are desired. Features: Average particle size of less than 5 microns provide high strength and is resistant to damage. Developed for a balance of speed and fine finish creates precise parts without sacrificing productivity. High resistance to wear minimizes replacement needs and improves cost of ownership. Available for order as billets, semi-finished rods, blocks, and plates. Applications: Fine detailed electrodes. Minimum tapered cavities. Blind cavity work. IC Molds. Aerospace applications.

Information provided by Entegris POCO Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size <= 5.0 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71
Flexural Strength 11200 psi
Compressive Strength 16900 psi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00160 ohm-cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CPOCO401 / 268786

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.