MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Corning HPFS® 8655 ArF Grade High Purity Fused Silica
Categories: Ceramic; Glass; Optical

Material Notes: Glass code 8655 is a high purity non-crystalline silica glass with excellent optical qualities. Product characteristics include extraordinary low refractive index variations leading to state-of-the-art homogeneity values, low birefringence, exceptional transmittance from the deep ultraviolet through the infrared region, and an ultra-low thermal expansion coefficient.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 522kg/mm² (100 g load)
Tensile Strength 54.0 MPa
Modulus of Elasticity 73.00 GPa
Modulus of Rupture 0.0524 GPaabraded
Compressive Strength 1140 MPa
Bulk Modulus 35.9 GPa
Poissons Ratio 0.16
Shear Modulus 31.0 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.480 µm/m-°C
@Temperature -100 - 100 °C
 0.520 µm/m-°C
@Temperature 5.00 - 35.0 °C
 0.570 µm/m-°C
@Temperature 0.000 - 200 °C
Specific Heat Capacity 0.770 J/g-°C
Thermal Conductivity 1.38 W/m-K
Softening Point 1630 °C107.6 Poise
Annealing Point 1180 °C1013 Poise
Strain Point 1070 °C1014 Poise
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.433027
@Wavelength 2326.050 nm
22°C, 1 atm, N2
 1.44078
@Wavelength 1813.570 nm
22°C, 1 atm, N2
 1.450304
@Wavelength 1014.26 nm
22°C, 1 atm, N2
 1.453731
@Wavelength 780.237 nm
22°C, 1 atm, N2
 1.456425
@Wavelength 656.454 nm
22°C, 1 atm, N2
 1.457077
@Wavelength 632.990 nm
22°C, 1 atm, N2
 1.458522
@Wavelength 587.725 nm
22°C, 1 atm, N2
 1.463561
@Wavelength 480.126 nm
22°C, 1 atm, N2
 1.471446
@Wavelength 388.975 nm
22°C, 1 atm, N2
 1.479824
@Wavelength 334.244 nm
22°C, 1 atm, N2
 1.491056
@Wavelength 289.444 nm
22°C, 1 atm, N2
 1.523018
@Wavelength 226.572 nm
22°C, 1 atm, N2
 1.542731
@Wavelength 206.266 nm
22°C, 1 atm, N2
 1.575091
@Wavelength 184.950 nm
22°C, 1 atm, N2
Abbe Number 67.6Ve
 67.8Vd
Optical Dispersion 0.006797nF'-nC'
Transmission, Visible >= 99 %
@Wavelength 375 - 800 nm
IR Transmittance 0.00 %
@Wavelength 4300 nm
 12 %
@Wavelength 4000 nm
 70 %
@Wavelength 3500 nm
 87 %
@Wavelength 3000 nm
 98 %
@Wavelength 2500 nm
 >= 99 %
@Wavelength 1500 nm
 >= 99 %
@Wavelength 1000 nm
 >= 99 %
@Wavelength 2000 nm
UV Transmittance >= 99.75 %
@Wavelength 193 nm
Internal Transmission Ti = 99.75 %/mm @193 nm.
 
Descriptive Properties
Birefringence < 1 (nm/cm)(lower upon request)
Homogeneity GradeAA, A, C, F
Inclusion Class0, 1, 2
Metallic Impurities< 10 ppb
OH Content< 1 ppm
Optical Stress Coefficient35.0 nm/cm MPa
Striae Class5ISO 10110-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CCORNG09x / 281583

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.