MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraiburg TPE THERMOLAST® M TM6ADT Thermoplastic Elastomer (MC/AD1 Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The MC/AD1 series is a material solution for applications requiring basic medical approvals such as ISO 10993-5. The series is characterized by its adhesion properties to polar thermoplastics such as ABS, PC and PET/PETG. The compounds are available in natural colors and can be colored in many different ways. The compounds are produced exclusively on a special medical unit.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Natural
Typical applications:
  • Seals
  • Flexible Connections
  • Membranes
  • Soft touch application (e.g. handles or push buttons)
  • Valves
Material advantages:
  • Adhesion to PC, ABS, PC/ABS, ASA, SAN
  • Adhesion to PET and PETG
  • Adhesion to PS
  • Sterilizable (autoclave 134°C, ß-/y-radiation 2x35 kGy, EtO)
  • Soft touch surface
  • Free from animal ingredients
  • KRAIBURG TPE Medical Service Package
  • US DMF listed

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5959DIN ISO 48-4
Tensile Strength 6.50 MPa943 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 650 %650 %200 mm/min; DIN 53504/ISO 37
Tear Strength 12.0 kN/m68.5 pliISO 34-1 Method B (b)
Compression Set  18 %
@Temperature 23.0 °C,
Time 259000 sec
18 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1 Method A
 40 %
@Temperature 70.0 °C,
Time 86400 sec
40 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1 Method A
 
Descriptive Properties
Adhesion to ABS4.5 N/mm (D)VDI 2019 two-component injection
Adhesion to PC4.5 N/mm (D)VDI 2019 two-component injection
Adhesion to PETG4.5 N/mm (D)VDI 2019 two-component injection
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8388 / 309052

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.