MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi FGF CARBON-P PET-G, 15% Carbon Fiber Filled 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PETG Copolyester

Material Notes: CARBON-P is a 15% carbon fiber reinforced PET-G based material. The result is a more than twice as stiff filament as PET-G with increased impact and heat resistance. This, together with other features, such as a matt surface, no warp, dimensionally stable and extremely forgiving to print, makes CARBON-P suitable for a very wide variety of applications.

Material features:

  • 15% Carbon fiber reinforced PET-G
  • Extremely stiff
  • Increased impact
  • No warping and dimensionally stable
  • Matt surface
  • Abrasive
Colors: Colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccISO 1183
Linear Mold Shrinkage 0.0016 cm/cmISO 294
Melt Flow 3.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaISO 527
Tensile Strength, Yield 101 MPaISO 527
Elongation at Break 3.7 %ISO 527
Elongation at Yield 2.7 %ISO 527
Tensile Modulus 9930 MPaISO 527
Charpy Impact, Notched 7.00 kJ/m²ISO 1791eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 73.0 µm/m-°CISO 11359
Vicat Softening Point 75.0 °CISO 306 B50
 
Processing PropertiesOriginal ValueComments
Zone 1 200 - 240 °C
Zone 2 225 - 265 °C
Zone 3 200 - 240 °C
Die Temperature 200 - 240 °C
Drying Temperature 70.0 °C<200 ppm
Dry Time 6.00 hour
 
Descriptive Properties
Mass Temperature218°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9806 / 301031

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.