System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LEXAN™ Copolymer XHT3146 Polycarbonate (PC) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
XHT3146 is a high mold release version of XHT3141 high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Features: High Heat Resistance
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.20
g/cc
1.20
g/cc
ASTM D792
Density
1.20
g/cc
0.0434
lb/in³
ISO 1183
Moisture Absorption
0.0200 %
0.0200 %
Injection Molding
0.300 %
0.300 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
0.30 %
0.30 %
ISO 62-1
Viscosity
16
cP
@Load 1.20 kg,
Temperature 300 °C
16
cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
30
cP
@Load 2.16 kg,
Temperature 330 °C
30
cP
@Load 4.76 lb,
Temperature 626 °F
MVR cc/10 min; ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
55.0
MPa
7980
psi
50 mm/min; ASTM D638
60.0
MPa
8700
psi
50 mm/min; ISO 527
Tensile Strength, Yield
70.0
MPa
10200
psi
50 mm/min; ASTM D638
70.0
MPa
10200
psi
50 mm/min; ISO 527
Elongation at Break
70 %
70 %
50 mm/min; ASTM D638
70 %
70 %
50 mm/min; ISO 527
Elongation at Yield
6.0 %
6.0 %
50 mm/min; ASTM D638
6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus
2.50
GPa
363
ksi
1 mm/min; ISO 527
2.70
GPa
392
ksi
50 mm/min; ASTM D638
Flexural Strength
80.0
MPa
11600
psi
yield, 2 mm/min; ISO 178
120
MPa
17400
psi
yld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2.50
GPa
363
ksi
2 mm/min; ISO 178
2.60
GPa
377
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
97.0
J
71.5
ft-lb
ASTM D256
55.0
J
@Temperature -30.0 °C
40.6
ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO)
9.00
kJ/m²
4.28
ft-lb/in²
80*10*3; ISO 180/1A
9.00
kJ/m²
@Temperature -30.0 °C
4.28
ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
NB
80*10*3; ISO 180/1U
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched
NB
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
1.10
J/cm²
5.23
ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
0.900
J/cm²
@Temperature -30.0 °C
4.28
ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
68.0
J
50.2
ft-lb
ASTM D3763
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity
0.200
W/m-K
1.39
BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi)
164
°C
327
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
166
°C
@Thickness 3.20 mm
331
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
152
°C
306
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
156
°C
@Thickness 3.20 mm
313
°F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point
168
°C
334
°F
Rate B/50; ISO 306
170
°C
338
°F
Rate B/50; ASTM D1525
170
°C
338
°F
Rate B/120; ISO 306
Processing Properties
Metric
English
Comments
Nozzle Temperature
285
-
345
°C
545
-
653
°F
Zone 2
280
-
340
°C
536
-
644
°F
Zone 3
290
-
350
°C
554
-
662
°F
Melt Temperature
290
-
350
°C
554
-
662
°F
Injection Molding
Mold Temperature
95.0
-
130
°C
203
-
266
°F
Drying Temperature
135
°C
275
°F
Injection Molding
Dry Time
4.00
-
6.00
hour
4.00
-
6.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
43.5
-
102
psi
Shot Size
40 - 60 %
40 - 60 %
Vent Depth
0.00250
-
0.00800
cm
0.000984
-
0.00315
in
Screw Speed
40
-
90
rpm
40
-
90
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH80462 / 288409
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.