MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Epoxies, Etc 10-3041 Fast Curing Toughened Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: 10-3041 is a toughened industrial grade epoxy adhesive. Once mixed, the adhesive forms structural bonds quickly and is tack free within thirty minutes. A 3,000 psi lap shear strength (aluminum to aluminum) is achieved within four hours. 10-3041 provides a unique combination of high lap shear strength, high peel resistance and impact endurance. Once fully cured, the epoxy adhesive is also resistant to a wide range of chemicals and solvents. The adhesive also offers higher heat performance than most fast setting epoxies. The medium viscosity of the 10-3041 allows for easy application. It is packaged in the easy to use TriggerBond® dispensing system. 10-3041 is low in odor and cures under a wide range of temperatures and humidity levels. The high performance epoxy adhesive forms excellent bonds to a wide variety of plastics and metals. It acts as an outstanding electrical insulator and therefore suitable for many electronic bonding applications.

Features:

  • Fast room temperature cure
  • Low odor (no mercaptan functionality)
  • Packaged in TriggerBond® system
  • Forms strong bonds to a variety of substrates
  • Electrically insulating
  • Vibration and impact resistant

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccHardener
 1.14 g/cc1.14 g/ccResin
Viscosity 7000 cP7000 cPHardener
 25000 cP25000 cPResin
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  60
@Temperature 60.0 °C
60
@Temperature 140 °F
 80
@Temperature 25.0 °C
80
@Temperature 77.0 °F
Shear Strength  20.7 MPa
@Time 14400 sec
3000 psi
@Time 4.00 hour
Lap (AL/AL)
 23.8 MPa
@Time 86400 sec
3450 psi
@Time 24.0 hour
Lap (AL/AL)
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.40e+12 ohm-cm2.40e+12 ohm-cm
Dielectric Constant 5.3
@Frequency 100 Hz
5.3
@Frequency 100 Hz
Dielectric Strength 17.3 kV/mm440 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  <= 40.0 min
@Temperature 65.0 °C
<= 0.667 hour
@Temperature 149 °F
 120 - 240 min
@Temperature 25.0 °C
2.00 - 4.00 hour
@Temperature 77.0 °F
Gel Time 12.0 min
@Load 0.00500 kg
12.0 min
@Load 0.0110 lb
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorClearHardener
 Off-WhiteMixed
 Off-WhiteResin
Mix Ratio2:1by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX079 / 316756

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.