Appearance: Blue Paste Product Benefits: - Electrically Insulating
- Solvent-free
- Low viscosity
Cure: Heat cureApplication: Electrically insulating adhesive Application Method: Stamping or Syringe dispensing LOCTITE ABLESTIK 84-3LV adhesive is designed for die attach applications. LOCTITE ABLESTIK 84-3LV adhesive is a low viscosity version of LOCTITE ABLESTIK 84-3 adhesive. Information provided by Loctite® |