MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Pressure Seal 9717 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9717 is a 70 durometer black colored Fluorinated Hydrocarbon elastomer, it is formulated with molybdenum disulfide to provide internal lubrication. It exhibits good resistance to compression set, petroleum based oils, aliphatic and aromatic fuels.

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.96 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73
 64
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 65
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 69
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 70
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 70
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 70
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 73
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 73
@Temperature 250 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1746 psi
 1194.3 psi
@Temperature 250 °C,
Time 252000 sec
Heat Aged
 1396.8 psi
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 1485.8 psi
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 1594.1 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 1686.7 psi
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 1690.1 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 1796.3 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
Elongation, Ultimate 288 %
 262.9 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 262.9 %
@Temperature 200 °C,
Time 252000 sec
Stauffer Blend 7700
 275 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 275 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 288 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 288 %
@Temperature 200 °C,
Time 252000 sec
Service Fluid 101
 362.9 %
@Temperature 250 °C,
Time 252000 sec
Heat Aged
100% Modulus 648 psi
Tear Strength 0.000 pliDie B
Compression Set 4.7 %
@Temperature 23.0 °C,
Time 79200 sec
Plied
 19.5 %
@Temperature 200 °C,
Time 79200 sec
Plied
 26 %
@Temperature 175 °C,
Time 79200 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -6.00 °F
Shrinkage 0.10 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 0.30 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 1.5 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 4.3 %
@Temperature 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 6.0 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 12.8 %
@Temperature 200 °C,
Time 252000 sec
Volume, Service Fluid 100
 32.5 %
@Temperature 200 °C,
Time 252000 sec
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL117 / 318327

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.