MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ SD000 PA12  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccASTM D792
Density 1.124 g/ccASTM D792
Moisture Absorption 0.150 %50% RH, 24 hrs; ASTM D570
 0.210 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow >= 0.020 cm/cm
@Time 86400 sec
ASTM D955
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm
@Time 86400 sec
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaType I, 5 mm/min; ASTM D638
 44.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 49.0 MPa5 mm/min; ISO 527
 51.0 MPaType I, 5 mm/min; ASTM D638
Elongation at Break 17.1 %5 mm/min; ISO 527
 28.1 %Type I, 5 mm/min; ASTM D638
Elongation at Yield 11.3 %5 mm/min; ISO 527
 13.4 %Type I, 5 mm/min; ASTM D638
Tensile Modulus 2100 MPa1 mm/min; ISO 527
 2210 MPa5 mm/min; ASTM D638
Flexural Strength 67.0 MPaISO 178
Flexural Modulus 1980 MPa2 mm/min; ISO 178
 2050 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 35.0 J/mASTM D256
Izod Impact, Unnotched 1910 J/mASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 219 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 2.00 J
@Temperature 23.0 °C
ASTM D3763
Impact Test 1.00 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.0 - 4.0 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 99.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
CTE, linear, Transverse to Flow 108 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 137 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 158 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 96.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI52011 / 152057

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.