MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX4610 Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 4610 resin is a 10% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This high performance injection moldable grade has a UL 5VA flame rating, non-brominated / non-chlorinated FR package, UL746C Outdoor Suitability rating of F1, excellent chemical resistance, high heat resistance, high flow, and is laser weldable. NORYL GTX4610 resin is an excellent candidate for a wide variety of electrical applications including connectors, sockets, sensors, terminal blocks and insulator components. NORYL GTX™ 4610 resin is also an excellent candidate for electric vehicle (EV) battery applications including housings and covers.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Flame Retardant,Good Stiffness,Weatherable,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Density 1.21 g/ccISO 1183
Moisture Absorption 0.0700 %Injection Molding
 0.500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.8 %ISO 62-1
Viscosity 15 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0088 - 0.0094 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0095 - 0.0101 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 18 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 88.0 MPa5 mm/min; ASTM D638
 88.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 88.0 MPa5 mm/min; ASTM D638
 88.0 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ISO 527
Elongation at Yield 3.0 %5 mm/min; ISO 527
Tensile Modulus 5000 MPa5 mm/min; ASTM D638
 5000 MPa1 mm/min; ISO 527
Flexural Strength 145 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 145 MPayield, 2 mm/min; ISO 178
Flexural Modulus 4600 MPa1.3 mm/min, 50 mm span; ASTM D790
 4600 MPa2 mm/min; ISO 178
Izod Impact Notched 80.0 JASTM D256
 65.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Charpy Impact, Notched 5.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 12.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Strength 23.2 kV/mm
@Thickness 1.60 mm
in air; ASTM D149
 24.4 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
 425 VIEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.800 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 41.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 41.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 224 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 220 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 218 °CRate B/50; ASTM D1525
 218 °CRate B/50; ISO 306
 220 °CRate B/120; ISO 306
UL RTI, Electrical 140 °CUL 746B
UL RTI, Mechanical with Impact 100 °CUL 746B
UL RTI, Mechanical without Impact 140 °CUL 746B
Flammability, UL94 V-1
@Thickness >=0.800 mm
UL 94
 V-0
@Thickness >=1.50 mm
UL 94
 5VA
@Thickness >=2.00 mm
UL 94
Glow Wire Ignition Temperature 800 °C
@Thickness 1.00 mm
IEC 60695-2-13
 800 °C
@Thickness 1.50 mm
IEC 60695-2-13
 800 °C
@Thickness 2.00 mm
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 800 °C
@Thickness 1.00 mm
IEC 60695-2-12
 800 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 305 °C
Zone 2 270 - 305 °C
Zone 3 275 - 305 °C
Melt Temperature 280 - 305 °CInjection Molding
Mold Temperature 75.0 - 120 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82116 / 290063

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.