Krytox™ 2C grease is made using Krytox™ PTFE and a non-melting thickener. Krytox™ 2C greases contain an oil-soluble additive that is effective at preventing corrosion and reducing wear. It also contains a micro-powder, boron nitride, extreme pressure additive. Typical applications include those in potentially corrosive atmospheres, where vibrational or shock loading may be significant and an element will spend more time experiencing mixed film or boundary lubrication versus the desired full film or hydrodynamic lubrication. Anti-corrosion additive. Anti-wear additive. Extreme pressure additive.Information provided by Chemours Krytox |