Product Description: Multi-Filament; Characteristics: Controlled rheology, Good softness, Anti gas-fading Availability: Asia Pacific; Europe; North America Features: Controlled Rheology; Gas-fading Resistant; Homopolymer; Soft Uses: Filaments Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520© 3.1a RoHS Compliance: RoHS Compliant UL File Number: E162823 Processing Method: Filament ExtrusionInformation provided by Formosa Chemicals & Fiber Corporation |