MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A 246M Natural Nylon 66, Impact Modified, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Product Description: Ultramid® A 246M Natural is an unfilled polyamide 6.6, impact modified, for injection molding. This grade offers an excellent impact resistance, even at a low temperature.

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Additive: Impact Modifier

Features: Good Mold Release; High Impact Resistance; Low Temperature Impact Resistance

Use: Automotive Applications; Consumer Applications; Footwear; Outdoor Applications; Power/Other Tools; Sporting Goods

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Maximum Moisture Content 0.200.20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiISO 527-2
Tensile Strength, Yield 42.0 MPa6090 psiISO 527-2
Elongation at Yield 210 %210 %ISO 527-2/50
Tensile Modulus 0.600 GPa87.0 ksiISO 527-1
Flexural Strength 27.0 MPa3920 psiISO 178
Flexural Modulus 0.703 GPa102 ksiISO 178
Izod Impact, Notched 1.23 J/cm2.30 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 79.8 kJ/m²38.0 ft-lb/in²ISO 180/A
Charpy Impact, Notched 10.1 J/cm²48.0 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 62631-3-2
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 265 - 275 °C509 - 527 °F
Middle Barrel Temperature 270 - 280 °C518 - 536 °F
Front Barrel Temperature 280 - 285 °C536 - 545 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2079 / 310772

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.