System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LEXAN™ Copolymer XHT4141 Polycarbonate (PC) (Europe)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Features: High Heat Resistance
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.20
g/cc
ASTM D792
Density
1.21
g/cc
ISO 1183
Moisture Absorption
0.0200 %
Injection Molding
0.250 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation
0.50 %
ISO 62-1
Viscosity
24
cP
@Load 2.16 kg,
Temperature 330 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0060
-
0.0095
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
25
g/10 min
@Load 2.16 kg,
Temperature 330 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
67.0
MPa
50 mm/min; ISO 527
69.0
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
77.0
MPa
50 mm/min; ASTM D638
78.0
MPa
50 mm/min; ISO 527
Elongation at Break
50 %
50 mm/min; ASTM D638
50 %
50 mm/min; ISO 527
Elongation at Yield
7.0 %
50 mm/min; ASTM D638
7.0 %
50 mm/min; ISO 527
Tensile Modulus
2730
MPa
5 mm/min; ASTM D638
2750
MPa
1 mm/min; ISO 527
Flexural Strength
80.0
MPa
yield, 2 mm/min; ISO 178
120
MPa
yld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2600
MPa
1.3 mm/min, 50 mm span; ASTM D790
2600
MPa
2 mm/min; ISO 178
Izod Impact Notched
93.0
J
ASTM D256
76.0
J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO)
10.0
kJ/m²
80*10*3; ISO 180/1A
8.00
kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
80*10*3; ISO 180/1U
NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched
NB
Edgew 80*10*3 sp=62mm; ISO 179/1eU
NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
11.0
kJ/m²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
9.00
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
72.0
J
ASTM D3763
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+17
ohm-cm
ASTM D257
Surface Resistance
>=
1.00e+17
ohm
ASTM D257
Dielectric Constant
3.02
@Frequency 1e+6 Hz
ASTM D150
3.12
@Frequency 100 Hz
ASTM D150
Comparative Tracking Index
175
-
250
V
UL 746A
Hot Wire Ignition, HWI
15
-
30
sec
@Thickness 1.50 mm
UL 746A
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness 1.50 mm
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
60.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity
0.200
W/m-K
ASTM C177
Hot Ball Pressure Test
125
°C
PASS; IEC 60695-10-2
165
°C
PASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
173
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
174
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
162
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
165
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point
181
°C
Rate B/120; ISO 306
183
°C
Rate B/50; ISO 306
183
°C
Rate B/50; ASTM D1525
UL RTI, Electrical
150
°C
UL 746B
UL RTI, Mechanical with Impact
130
°C
UL 746B
UL RTI, Mechanical without Impact
150
°C
UL 746B
Flammability, UL94
HB
@Thickness >=1.50 mm
UL 94
Glow Wire Ignition Temperature
875
°C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Thickness 1.00 mm
IEC 60695-2-12
960
°C
@Thickness 2.00 mm
IEC 60695-2-12
960
°C
@Thickness 3.00 mm
IEC 60695-2-12
Processing Properties
Original Value
Comments
Nozzle Temperature
295
-
340
°C
Zone 2
290
-
335
°C
Zone 3
300
-
345
°C
Melt Temperature
300
-
345
°C
Injection Molding
Mold Temperature
95.0
-
130
°C
Drying Temperature
135
°C
Injection Molding
Dry Time
4.00
-
6.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
Shot Size
40 - 60 %
Vent Depth
0.00250
-
0.00800
cm
Screw Speed
40
-
90
rpm
Descriptive Properties
Metallized Haze Onset
175 °C
SABIC method
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH80468 / 288415
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.