MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
DowAksa CarbonBond™ 300-UW Saturant Epoxy Resin System
Categories: Polymer; Thermoset; Epoxy

Material Notes: DowAksa CarbonBond™ 300-UW Saturant Resin System is a fast-setting, general purpose epoxy laminating and bonding resin system that is well suited for use in performing repairs to various submerged structures or facilities in a freshwater or salt water environment. It has been found particularly useful in performing field repairs of pipes, poles, piles, tanks and other structures requiring a very fast set up and cure in the presence of water. The system may be used in high humidity situations and will cure in the presence of moisture.

Information provided by DowAksa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 lb/galPart B
 9.60 lb/galPart A
Viscosity 1200 cPPart A
 1500 cPMixed
 2100 cPPart B
Linear Mold Shrinkage 0.0080 in/inASTM D2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88ASTM D2240
Tensile Strength 9.60 ksi14 Day Cure; ASTM D638
Elongation at Break 2.3 %14 Day Cure; ASTM D638
Tensile Modulus 416 ksi14 Day Cure; ASTM D638
Flexural Strength <= 14.8 ksi14 Day Cure; ASTM D790
Flexural Modulus 427 ksiASTM D790
Compressive Strength 15.9 ksiASTM D695
Izod Impact, Notched 1.38 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °FHDT load not reported, RT Cure
 200 °FHDT load not reported, Post-Cured
 
Processing PropertiesOriginal ValueComments
Gel Time 18.0 min150g
 
Descriptive Properties
ColorAmberMixed
Mix Ratio100:22 A:BWeight
 4.2:1 A:BVolume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWAK992 / 287939

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.