MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Go Yen Chemical GGK-1480 Water-Based Scratch & Wear Resistance Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: As we know that water-based and environmental friendly material is a trend in the future, besides users are searching for a product which can supply antiscratch and anti-wear functions for water-based paint and resin products. In order to reflect and meet customer’s request, GO YEN CHEMICAL INDUSTRIAL CO. LTD. (GYC Group) specializes in water-based additive field and develops scratch& wear resistance agent for different stages of production. GGK-1480 water-based scratch & wear resistance agent is suitable for all kinds of water-based resin, ink and paint industry. The product can be easily added into water-based resin ink and paint. Besides, the product also can be used to alcohol and other polar solvent resin system. GGK-1480 provides good wear & scratch resistance, antilaminating, smoothness and glossiness properties for products.

Advantages:

  • Improve wear resistance for product
  • Few of dosage, High Price-performance ratio
  • Scratch resistance effect
  • Provide excellent smoothness and wetting properties for products
  • Increase coating mobility
  • Increase coating smoothness property
  • Lower surface tension
  • Good compatibility with various water-based ink and paint
Applications:
  • Various water based resin
  • Aquaous Acrylic
  • Water-based PU (WBPU)
  • Epoxy resin
  • Water-based ink
  • Water-based coating
  • Hydrophilic products
  • Latex paint
  • Water- based leather finishing agent
  • Can be used to alcohol or other polar solvent resin system

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³
 
Descriptive Properties
AppearanceLiquid
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN309 / 266617

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.