MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Kynar Flex® 3030-50 PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes:

Information provided by Arkema Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 - 1.82 g/cc1.78 - 1.82 g/ccASTM D792
Water Absorption <= 0.050 %<= 0.050 %ASTM D570
Viscosity 2.10e+6 - 3.00e+6 cP
@Shear Rate 100 1/s,
Temperature 230 °C
2.10e+6 - 3.00e+6 cP
@Shear Rate 100 1/s,
Temperature 446 °F
Melt; ASTM D3835
Melt Flow 2.5 - 7.5 g/10 min
@Load 12.5 kg,
Temperature 230 °C
2.5 - 7.5 g/10 min
@Load 27.6 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 6050 - 60ASTM D2240
Tensile Strength at Break 18.6 - 24.1 MPa2700 - 3500 psiASTM D638
Tensile Strength, Yield 11.7 - 15.9 MPa1700 - 2310 psiASTM D638
Elongation at Break <= 500 %<= 500 %ASTM D638
Elongation at Yield 25 - 40 %25 - 40 %ASTM D638
Tensile Modulus 0.207 - 0.345 GPa30.0 - 50.0 ksiASTM D638
Flexural Modulus 0.248 - 0.303 GPa36.0 - 43.9 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Taber Abrasion, mg/1000 Cycles 28 - 3328 - 33CS 17 1000g:pad; ASTM-G195-13A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.80e+13 - 8.00e+13 ohm-cm7.80e+13 - 8.00e+13 ohm-cm65% R.H; ASTM D257
Surface Resistivity per Square 7.60e+11 - 7.90e+11 ohm7.60e+11 - 7.90e+11 ohmASTM D257
Dielectric Strength 1.00 - 1.20 kV/mm25.4 - 30.5 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 153 - 194 µm/m-°C85.0 - 108 µin/in-°FASTM D696
Melting Point 160 - 168 °C320 - 334 °FASTM D3418
Maximum Service Temperature, Air 150 °C302 °FUL RTI
Glass Transition Temp, Tg -40.0 °C-40.0 °FASTM D7028
Oxygen Index >= 43 %>= 43 %
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARKF714a / 291162

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.