MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes:

Data provided by Clariant Masterbatches

Key Words: PBT
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Water Absorption 0.080 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.018 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 8500 psiASTM D638
Elongation at Break 50 %ASTM D638
Flexural Yield Strength 11000 psiASTM D790
Flexural Modulus 330000 psiASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 310 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 153 °FASTM D648
Flammability, UL94 HB
@Thickness 0.7937 - 6.35 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 430 - 480 °F
Middle Barrel Temperature 440 - 490 °F
Front Barrel Temperature 450 - 500 °F
Nozzle Temperature 460 - 510 °F
Melt Temperature 450 - 475 °F
Mold Temperature 150 - 180 °F
Injection Pressure 720 - 1200 psiSecondary
 1200 - 2000 psiInitial
Back Pressure 50.0 - 100 psi
Shot Size 30 - 80 %
Screw Speed 25 - 80 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Renol PCSP0006 Polycarbonate, Laser Markable
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity
Gromax PBT 1100-211L
Chem Polymer Durlex 740 G PBT, 40% Short Glass Fiber Reinforced
Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced

PCLAR138 / 82263

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.