MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-3287A TPU Water Vapor Transmission Grade
Categories: Polymer; Thermoplastic

Material Notes: In order to respond customer’s request about water -proof TPU, GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC Group) especially designs moisture vapor transmission grade of TPU. The grade has high moisture vapor transmission, high water pressure resistance, good formability, suitable for water- proof permeability of film processing, extrusion and blown field.

Advantages:

  • Excellent moisture vapor transmission
  • High water pressure resistance
  • Good formability
  • Water-proof ability
  • Improve added-value of products
Application: Blown

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 4000 g/m²/dayASTM E-96BW
 >= 7000 g/m²/dayASTM E-96BW
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80 - 84
Elongation at Break 500 - 800 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 195 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN709 / 267017

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.