MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ GTX840 PPE+PA66 (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: 40% glass filled PPE+PA66 blend for automotive under-the-hood and FLEN applications

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Density 1.45 g/ccISO 1183
Moisture Absorption 0.100 %23°C / 50% RH; ISO 62
Moisture Absorption at Equilibrium 0.30 %ASTM D570
Linear Mold Shrinkage, Flow 0.0024 - 0.0027 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0063 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 220 °C
MVR, cm^3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength at Break 178 MPaType I, 5 mm/min; ASTM D638
 198 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ISO 527
 2.0 %Type I, 5 mm/min; ASTM D638
Flexural Yield Strength 249 MPa1.3 mm/min, 50 mm span; ASTM D790
 280 MPa2 mm/min; ISO 178
Flexural Modulus 11860 MPa1.3 mm/min, 50 mm span; ASTM D790
 12270 MPa2 mm/min; ISO 178
Izod Impact, Notched 94.0 J/mASTM D256
 90.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 11.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Tangent Modulus 13520 MPa5 mm/min; ASTM D638
 13940 MPa1 mm/min; ISO 527
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 - 19.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 90.0 - 93.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 258 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 260 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 244 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 247 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 246 °CRate B/120; ISO 306
 246 °CRate B/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 295 - 315 °C
Zone 1 275 - 315 °C
Zone 2 280 - 315 °C
Zone 3 290 - 315 °C
Melt Temperature 295 - 315 °C
Mold Temperature 75.0 - 120 °C
Drying Temperature 95.0 - 105 °C
Dry Time 3.00 - 4.00 hour
 8.00 hourCumulative
Moisture Content 0.070 %
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 70G43L NC010 PA66-GF43
Akro-Plastic Akroloy® PA GF 60 natural (2941) PA 66 + PA 6I/6T Dry, 60% Glass Filled
Akro-Plastic Akroloy® PA GF 60 natural (2941) PA 66 + PA 6I/6T Conditioned, 60% Glass Filled
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled

PSABI22395 / 215531

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.