LNP STAT-KON DE0026 compound is based on Polycarbonate (PC) resin containing 10% carbon fiber. Added features of this grade include: Non-Brominated, Non-Chlorinated Flame Retardant, Electrically Conductive. Features: Light-weight Structural,Super Strong (Carbon Fiber Filled),Flame Retardant,Non-Chlorinated,Non-Brominated,Electrically Conductive Information provided by SABIC |