MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® 1202K Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Formolene® 1202K is a high molecular weight, polypropylene homopolymer designed for biaxially oriented film (BOPP). It has been designed for improved processability in the orientation process, which also results in better end use performance than existing grades. It does not contain slip or antiblock. Formolene® 1202K meets the requirements of the US FDA as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact. This material is free of animal-derived content.

Availability: North America

Features: Food Contact Acceptable; Good Processability; High Molecular Weight; Homopolymer; No Animal Derived Components

Uses: Bi-axially Oriented Film

Agency Ratings: EC 1907/2006 (REACH); FDA 21 CFR 177.1520

Form: Pellets

Processing Method: Bi-axially Oriented Film

Information provided by Formosa Plastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104Injection Molded; ASTM D785
Tensile Strength, Yield 4930 psiInjection Molded, 2.0 in/min; ASTM D638
Elongation at Yield 10 %Injection Molded, 2.0 in/min; ASTM D638
Flexural Modulus 200000 psi1% Secant, Injection Molded, 0.051 in/min; ASTM D790
Izod Impact, Notched 0.510 ft-lb/inInjection Molded; ASTM D256A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFPCR744 / 311437

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.