LNP THERMOCOMP MC004 compound is based on Polypropylene (PP) resin containing 20% carbon fiber. Added features of this grade include: Electrically Conductive. Features: High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Electrically Conductive,Structural Information provided by SABIC |