MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

North American Loblolly Pine Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Pinus Taeda; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.500 g/cc0.0181 lb/in³Oven Dry Weight/Unseasoned Volume
 0.865 g/cc0.0312 lb/in³Unseasoned*
Cell Length 3.60 mm0.142 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1800 N405 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2000 N450 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 3100 N697 lb (f)Side
Tensile Strength, Ultimate 1.93 MPa280 psiPerpendicular to Grain*
 3.20 MPa464 psiPerpendicular to Grain
Modulus of Rupture 0.0517 GPa7.50 ksiStatic Bending*
 0.0880 GPa12.8 ksiStatic Bending
Flexural Yield Strength 30.3 MPa4400 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 9.51 GPa1380 ksiStatic Bending*
 12.42 GPa1801 ksiStatic Bending
Compressive Strength 3.79 MPa550 psiPerpendicular to Grain*
 6.80 MPa986 psiPerpendicular to Grain
 19.8 MPa2870 psiParallel to Grain*
 24.7 MPa3580 psiMax Crushing Strength Parallel to Grain*
 49.0 MPa7110 psiParallel to Grain
Poissons Ratio 0.2920.292µLT, 12% Moisture Content
 0.3280.328µLR, 12% Moisture Content
 0.3620.362µTR, 12% Moisture Content
 0.3820.382µRT, 12% Moisture Content
Shear Strength 6.21 MPa900 psiParallel to Grain*
 9.40 MPa1360 psiOrientation Unknown
Impact 3.13.1in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 95009500psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00558 J/cm³0.810 in-lb/in³Static Bending*
Work to Maximum Load 0.0552 J/cm³8.00 in-lb/in³Static Bending*
Toughness 18.1 J13.3 ft-lbRadial
 29.5 J21.8 ft-lbTangential
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.124 W/m-K0.860 BTU-in/hr-ft²-°FOven Dry
 0.144 W/m-K1.00 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.8 %4.8 %Radial; Green to Zero Moisture
 7.4 %7.4 %Tangential; Green to Zero Moisture
 12.3 %12.3 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Pine Wood
Northern White Pine Wood
Southern Pine Wood
American Eastern White Pine Wood
American Longleaf Pine Wood

PTSA600 / 71267

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.