MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Chemicals NOCOLOK® Sil Flux (fine grade)
Categories: Ceramic

Material Notes: Reactive flux for brazing of aluminum and filler alloy generating flux for brazing aluminum.

Classifications: HS No.: 38109090 /CAS-No.: 60304-36-1

Composition: either 2:1: 66.6 % ± 1.5 % -NOCOLOK Flux and 33.3 % ± 1.5 % -Silicon powder or 3:1: 75% ± 1.5 % -NOCOLOK Flux and 25% ± 1.5 % -Silicon powder

Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electrical Appliances

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solubility in Water 0.45 %0.45 %NOCOLOK Flux
 
Thermal PropertiesMetricEnglishComments
Melting Point 564 - 572 °C1050 - 1060 °FNOCOLOK Flux
 
Descriptive Properties
Appearancegrey powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Verdant Specialty Solutions ALKAMULS® 504/V Surfactant
Syensqo (Solvay Specialty Polymers) Clearbreak 343 Demulsifier
Syensqo (Solvay Specialty Polymers) Cerox™ 2822 Surfactant
Syensqo (Solvay Specialty Polymers) Cerox™ 2610 Surfactant
Solvay SUPER CEROX™ 1663 Surfactant

WSOLV025 / 147674

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.