MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin EN185 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ EN185 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This extrusion grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of v0 at 3mm and V1 at 1.5mm. NORYL EN185 resin exhibits excellent impact strength, very low moisture absorption, good dimensional stability, and great machinability. NORYL EN185 resin is an excellent candidate for a variety of applications including fiber optic ducting,

Features: Hydrolytic Stability,Flame Retardant,Good Stiffness,Non-Halogenated,Non-Chlorinated,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Water Absorption 0.070 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Extrusion
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 113ASTM D785
Tensile Strength, Yield 42.0 MPa50 mm/min; ASTM D638
Elongation at Break 50 %50 mm/min; ASTM D638
Flexural Strength 67.0 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2270 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 389 JASTM D256
 160 J
@Temperature -40.0 °C
ASTM D256
Gardner Impact 13.0 J
@Temperature -40.0 °C
ASTM D3029
 24.0 J
@Temperature -30.0 °C
ASTM D3029
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.8
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 24.8 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0035
@Frequency 1e+6 Hz
IEC 60250
 0.0040
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
 >= 120 sec
@Thickness >=6.00 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 73.8 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Flammability, UL94 V-1
@Thickness >=1.50 mm
UL 94
 V-0
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 1 170 °CExtrusion
Zone 2 170 °CExtrusion
Zone 3 190 °CExtrusion
Zone 4 190 °CExtrusion
Adapter Temperature 205 °CExtrusion
Die Temperature 205 °CExtrusion
Melt Temperature 195 - 210 °CExtrusion
Drying Temperature 90.0 - 100 °CExtrusion
Dry Time 2.00 - 4.00 hourExtrusion
 8.00 hourCumulative; Extrusion
 
Descriptive Properties
Radiant Panel ListingTRUEUL Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82278 / 290225

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.