MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound OFL36 Polyphenylene Sulfide, Linear (PPS, Linear) (Asia)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP LUBRICOMP OFL36 compound is based on Polyphenylene Sulfide (PPS) - linear resin containing 30% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant,Structural

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccASTM D792
 1.70 g/ccISO 1183
Moisture Absorption 0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0400 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm24hrs; ASTM D955
 0.0013 - 0.0018 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0030 - 0.0048 cm/cm24hrs; ISO 294
 0.0030 - 0.0050 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 124 MPaISO 527
 145 MPaASTM D638
Elongation at Break 1.4 %ISO 527
 1.7 %ASTM D638
Tensile Modulus 11500 MPa1 mm/min; ISO 527
 12600 MPa50 mm/min; ASTM D638
Flexural Strength 197 MPaISO 178
 200 MPaASTM D790
Flexural Modulus 10950 MPaISO 178
 11030 MPaASTM D790
Izod Impact Notched 85.0 JASTM D256
Izod Impact, Unnotched 550 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 Jpeak; ASTM D3763
Impact Test 1.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.44ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.35ASTM D3702 Modified: Manual
K (wear) Factor 33.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 23.4 - 50.03 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 48.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 50.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 266 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 266 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 200 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.750 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 320 - 330 °C
Zone 3 330 - 345 °C
Melt Temperature 315 - 320 °CInjection Molding
Mold Temperature 140 - 165 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80923 / 288870

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.