MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

BASF Ultraform® W 2320 003 PRO AT POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product Description: Ultraform® W2320 003 PRO AT is a very easy flowing and rapidly freezing injection molding POM grade. This grade was developed for the medical device market. This grade complies with US Pharmacopeia: Biological Reactivity Tests, USP Plastic Class VI (USP VI), ISO 10993-5: Biological Evaluation of Medical Devices Part 5: Test for Cytotoxicity, DMF: A Drug Master File (DMF) has been registered at FDA for Ultraform® PRO and Food Contact: Ultraform® PRO is in compliance with multiple regional food contact regulations, especially for Europe and United States. Typical applications include functional parts in medical devices.

Availability: North America

Features: Food Contact Acceptable; Good Flow

Use: Medical/Healthcare Applications

Agency Ratings: DMF; EC 1907/2006 (REACH); FDA Food Contact; ISO 10993 Part 5; USP Class VI

RoSH Compliance: RoSH Compliant

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Water Absorption 0.20 %0.20 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.021 cm/cm0.021 in/inISO 294-4
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.0 MPa9430 psiISO 527-2
Elongation at Break 24 %24 %Nominal; ISO 527-2
Elongation at Yield 8.0 %8.0 %ISO 527-2
Tensile Modulus 2.85 GPa413 ksiISO 527-1
Izod Impact, Notched (ISO)  5.04 kJ/m²
@Temperature 22.8 °C
2.40 ft-lb/in²
@Temperature 73.0 °F
ISO 180
 5.04 kJ/m²
@Temperature -30.0 °C
2.40 ft-lb/in²
@Temperature -22.0 °F
ISO 180
Charpy Impact Unnotched  18.9 J/cm²
@Temperature 22.8 °C
90.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179
 18.9 J/cm²
@Temperature -30.0 °C
90.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched  0.399 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.441 J/cm²
@Temperature 22.8 °C
2.10 ft-lb/in²
@Temperature 73.0 °F
ISO 179
Tensile Creep Modulus, 1000 hours 1350 MPa196000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.0 µin/in-°FISO 11359-2
Melting Point 166 °C331 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature 80.0 - 110 °C176 - 230 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 3.50 - 7.03 MPa508 - 1020 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2118 / 310811

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.