MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® B27 HM 01 Nylon 6, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Product Description: Ultramid® B27 HM 01 is a low viscosity, heat stabilized, nylon 6 universal wire jacketing resin offering excellent performance through the range of THHN, THWN, AND TFFN constructions. It processes a balance of performance properties including flexibility, toughness and abrasion resistance combined with excellent chemical resistance to gasoline, oil and other hydrocarbons. It is a preferred resin for wire conductor jacketing, including shipboard cable, and non-metallic-shafted cable primary jacketing.

Availability: Europe; North America

Additive: Heat Stabilizer

Features: Abrasion Resistant; Chemical Resistant; Gasoline Resistant; Good Flexibility; Good Toughness; Heat Stabilized; Hydrocarbon Resistant; Low Viscosity; Oil Resistant

Use: Jacketing; Wire & Cable Applications

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Forms: Pellets

Processing Method: Wire & Cable Extrusion

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.660 g/ccApparent
Density 1.13 g/ccISO 1183
Water Absorption 2.7 %Equilibrium, 50% RH
Water Absorption at Saturation 9.5 %
Particle Size 2000 - 2500 µmPellet size, Cylindrical
Viscosity Measurement 136 - 15696% Sulfuric Acid (Sulphuric Acid); ISO 307
Viscosity Number 2.5 - 2.8 cm³/g1% in 96% Sulfuric Acid
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ISO 2039.2
Tensile Strength, Yield 11600 psiISO 527-2
Elongation at Yield 4.3 %ISO 527-2
Tensile Modulus 406000 psiISO 527-1
Flexural Modulus 377000 psiISO 178
Izod Impact, Notched (ISO) 1.00 ft-lb/in²
@Temperature -40.0 °C
ISO 180/A
 1.70 ft-lb/in²
@Temperature 22.8 °C
ISO 180/A
 
Thermal PropertiesOriginal ValueComments
Melting Point 428 °FISO 3146
 
Processing PropertiesOriginal ValueComments
Zone 1 464 - 491 °F
Zone 3 482 - 518 °F
Zone 5 500 - 554 °F
Moisture Content <= 0.17 %ISO 15512
 
Descriptive Properties
Extractables2.5-5.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2068 / 310761

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.