MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
OCSiAl TUBALL™ COAT E H2O 0.4% (DBD) BETA Suspension of graphene nanotubes
Categories: Carbon; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Versatile suspension of graphene nanotubes.

Benefits: Electrical conductivity, Mechanical performance, High transparency, Easy to handle, Retained rheological performance.

Applications: Acrylic, Adhesives, Binder, Coatings, Paints, Plastics, Primers, Printing Ink, PU, Suspension, Transparent Conductive Coatings, Transparent Films.

TUBALL™ COAT_E H2O 0.4% (distyryl biphenyl derivative) beta is a suspension of graphene nanotubes in water intended for reducing the surface electrical resistance of paint coatings produced from formulations based on water.

Applications: Waterborne construction and industrial coatings, automotive coatings, printing inks, coatings for wood materials, and adhesives. Uses in the plastics industry and in other applications are possible, including those related to electrical conductivity.

Information provided by OCSiAl

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.075 g/cc
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 98.8 %
 
Descriptive Properties
Distyryl Biphenyl Derivative Stabilizer (%)0.8
TUBALL™ Graphene Nanotubes (%)0.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EOCSIAL907 / 305646

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.