MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Notes: 25% Mineral - 15% Glass; Excellent stiffness and strength, especially at high temperatures, with improved warpage control over glass reinforced products; FMVSS Flammability: Passes, FMVSS 302

Features: Heat Stabilized

Processing Method: Injection Method

Forms: Pellets

Automotive Specifications: Chrysler Ms-DB41 CPN2554 Color: BK001 Black

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccASTM D792
Linear Mold Shrinkage 0.0015 - 0.0040 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 18500 psiASTM D638
Elongation at Break 2.5 %ASTM D638
Elongation at Yield 2.5 %ASTM D638
Flexural Strength 27500 psiASTM D790
Flexural Modulus 1.15e+6 psiASTM D790
Izod Impact, Notched 1.40 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 550 VUL 746
 
Thermal PropertiesOriginal ValueComments
Melting Point 495 °FDSC
Deflection Temperature at 1.8 MPa (264 psi) 465 °FUnannealed; ASTM D648
UL RTI, Electrical 149 °F
@Thickness 0.749 mm
UL 746
UL RTI, Mechanical with Impact 149 °F
@Thickness 0.749 mm
UL 746
UL RTI, Mechanical without Impact 149 °F
@Thickness 0.749 mm
UL 746
Flammability, UL94 HB
@Thickness 0.749 mm
Oxygen Index 24 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 465 - 495 °F
Middle Barrel Temperature 505 - 535 °F
Front Barrel Temperature 515 - 545 °F
Nozzle Temperature 515 - 540 °F
Melt Temperature 505 - 545 °FProcessing Temperature
Drying Temperature 175 °F
Moisture Content 0.20 %
 
Descriptive Properties
Suggested Regrind, max25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Teknor Apex Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced
Teknor Apex Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced
RTP Company RTP PA66 15 GF 25 M BLK Nylon 6/6 (PA), Value Product - 15% Glass Fiber - 25% Mineral - Heat Stabilized
Envalior Akulon® K224-HGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America)

PTEKNO435 / 128612

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.