MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Armeen 2C Dicocoalkylamines
Categories: Other Engineering Material

Material Notes: Armeen 2C is a dicocoalkylamine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.781 g/cc
@Temperature 80.0 °C
0.0282 lb/in³
@Temperature 176 °F
 0.787 g/cc
@Temperature 70.0 °C
0.0284 lb/in³
@Temperature 158 °F
 0.793 g/cc
@Temperature 60.0 °C
0.0286 lb/in³
@Temperature 140 °F
Viscosity  4.91 cP
@Temperature 60.0 °C
4.91 cP
@Temperature 140 °F
 40.1 cP
@Temperature 90.0 °C
40.1 cP
@Temperature 194 °F
 42.2 cP
@Temperature 80.0 °C
42.2 cP
@Temperature 176 °F
 45.4 cP
@Temperature 70.0 °C
45.4 cP
@Temperature 158 °F
Vapor Pressure <= 0.00133322 bar<= 0.999998 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 46.0 °C>= 115 °F
Boiling Point 180 °C
@Pressure 0.101325 MPa
356 °F
@Pressure 14.6921 psi
Flash Point >= 150 °C>= 302 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 2.00.00 - 2.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amine number140-155 mg KOH/g
Content= 6 %Primary Amine
 = 90 %Secondary Amine
 0-10 g I2/100 gIodine value
 361-401 g/eqNeutralization equivalent
Equivalent mass390 g/eq
HLB4.2Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY189 / 285712

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.