MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC GELOY™ CR7020 ASA (Americas)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: ASA. Profile and sheet. Excellent weatherability, good flow/aesthetics and high impact.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Moisture Absorption at Equilibrium 0.55 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 13 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 86ASTM D785
Tensile Strength at Break 34.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 41.0 MPa50 mm/min; ASTM D638
Elongation at Break 40 %50 mm/min; ASTM D638
Tensile Modulus 1790 MPa50 mm/min; ASTM D638
Flexural Yield Strength 58.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1790 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 320 J/mASTM D256
 58.0 J/m
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 25.0 JASTM D3763
Impact 10675Gardner Impact J/m (Procedure B); ASTM D4226
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+15 ohmASTM D257
Dielectric Constant 3.21
@Frequency 1e+6 Hz
ASTM D150
 5.2
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 15.9 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.026
@Frequency 1e+6 Hz
ASTM D150
 0.15
@Frequency 50.0 - 60.0 Hz
ASTM D150
Comparative Tracking Index >= 600 VUL 746A
Hot Wire Ignition, HWI 15 - 30 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 84.6 µm/m-°C
@Temperature -30.0 - 0.000 °C
ASTM E831
 86.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 91.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °Cannealed; ASTM D648
 76.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 79.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 99.0 °CRate B/50; ASTM D1525
UL RTI, Electrical 50.0 °CUL 746B
UL RTI, Mechanical with Impact 50.0 °CUL 746B
UL RTI, Mechanical without Impact 50.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.49 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Gloss 95 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Zone 1 205 - 215 °CProfile Extrusion
Zone 2 215 - 230 °CProfile Extrusion
Zone 3 220 - 240 °CProfile Extrusion
Zone 4 225 - 245 °CProfile Extrusion
Adapter Temperature 225 - 245 °CProfile Extrusion
Die Temperature 225 - 245 °CProfile Extrusion
Melt Temperature 225 - 255 °C
Drying Temperature 80.0 - 90.0 °CProfile Extrusion
Dry Time 3.00 - 6.00 hourProfile Extrusion
 12.0 hourCumulative; Profile Extrusion
Moisture Content >= 0.020 %
Precipitation Temperature 15.0 - 65.0 °CCalibrator
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10119 / 243586

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.