MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAFORM® AH UD blue POM-C
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes:
  • metal detectable
  • x-ray opaque
  • food grade blue
  • good mechanical properties
  • good machinability
Target Industries:
  • food processing
  • food technology
  • food engineering
  • engineering for beverage filling systems
  • conveyor technology
  • packaging and paper machinery
  • pharmaceutical industry
  • others

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.71 g/cc0.0618 lb/in³
Moisture Absorption 0.130 %
@Time 86400 sec
0.130 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8989ASTM D 785
Tensile Strength, Yield 51.7 MPa7500 psiASTM D 638
Elongation at Break 12 %12 %ASTM D 638
Modulus of Elasticity 2.07 GPa300 ksiASTM D 638
Flexural Strength 862 MPa125000 psiASTM D 790
Flexural Modulus 3.17 GPa460 ksiASTM D 790
Compressive Yield Strength 87.22 MPa
@Strain 10 %
12650 psi
@Strain 10 %
ASTM D 695
Compressive Strength 11.0 MPa
@Strain 1 %
1600 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 1.65 GPa240 ksiASTM D 695
Izod Impact, Unnotched 0.363 J/cm0.680 ft-lb/inASTM D 256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D 257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C12.0 µin/in-°FASTM D 696
Melting Point 165 °C329 °F
Maximum Service Temperature, Air 100 °C212 °FLong Term
 141 °C285 °FShort Term
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FASTM D 648
 
Descriptive Properties
Colordark blue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8160 / 319088

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.