MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Polymaker PolyLite™ ABS 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: PolyLite™ ABS is made with a specialty bulk-polymerized ABS resin, which has significantly lower volatile content compared to traditional ABS resins. It delivers excellent printing quality with minimal odor during printing.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183, GB/T 1033
Moisture Absorption at Equilibrium 0.35 %
@Temperature 23.0 °C
70% RH
Melt Flow 9.0 - 14 g/10 min
@Load 1.16 kg,
Temperature 220 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72
Tensile Strength 25.4 MPaZ Direction, Dry; ISO 527, GB/T 1040
 33.3 MPaX-Y Direction, Dry; ISO 527, GB/T 1040
Elongation at Break 2.4 %Z Direction, Dry; ISO 527, GB/T 1040
 2.7 %X-Y Direction, Dry; ISO 527, GB/T 1040
Modulus of Elasticity 1.835 GPaZ Direction, Dry; ISO 527, GB/T 1040
 2.174 GPaX-Y Direction, Dry; ISO 527, GB/T 1040
Flexural Strength 72.8 MPaX-Y Direction, Dry; ISO 178, GB/T 9341
Flexural Modulus 2844 MPaX-Y Direction, Dry; ISO 178, GB/T 9341
Charpy Impact, Notched 10.5 kJ/m²ISO 179, GB/T 1043
 12.6 kJ/m²ISO 179, GB/T 1043
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature 113.5 °C10°C/min; DSC
Deflection Temperature at 0.46 MPa (66 psi) 99.2 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 98.2 °CISO 75
Vicat Softening Point 103.9 °CISO 306, GB/T 1633
Glass Transition Temp, Tg 101.1 °C10°C/min; DSC
Decomposition Temperature >= 380 °C10°C/min; DSC
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 264 °C
 
Descriptive Properties
Bed temperature (°C)90 - 100
Build surface materialBuildTak®
Printing speed (mm/s)30-50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYMA973 / 291038

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.