MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SK Chemicals SKYPEL G140DW Engineering Thermoplastic Polyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: SKYPEL G is a standard grade thermoplastic elastomer with excellent heat resistance and mechanical strength.

Tensile property tests on ASTM Type IV dumbbells diecut from injection molded slab 2mm thick. Crosshead speed 50 mm/min.

Information provided by SK Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Water Absorption 0.60 %ASTM D570
Linear Mold Shrinkage 0.0080 cm/cmASTM D955
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40ASTM D2240
Tensile Strength at Break 26.5 MPaASTM D638
Tensile Stress at Strain 24.0 kg(f)/cm²
@Strain 5.0 %
ASTM D638
 44.0 kg(f)/cm²
@Strain 10 %
ASTM D638
Elongation at Break 680 %ASTM D638
Flexural Strength 66.7 MPaASTM D790
Resilience 57Vertical rebound; ASTM D2632
Izod Impact, Notched NB
@Thickness 6.35 mm
ASTM D256
Tear Strength 115 kN/m
@Thickness 2.00 mm
Crosshead speed 51mm/min; ASTM D1004
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+13 ohm-cmASTM D257
Surface Resistance 2.00e+14 ohmASTM D257
Dissipation Factor 0.054
@Frequency 1e+8 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 153 °CDSC Peak; 10°C/min.; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSK9916 / 291432

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.