Angst + Pfister developed and produced with PERTEC® UP FKM, UP meaning „Ultra Pure“, a new high tech compound within the PERTEC® family that is especially designed for applications where the pureness of the material is absolutely essential. This is especially the case within the food, pharma and medical industry where the human health can directly be affected. Therefore in those areas only material can be used that does not emit any substances or material that can contaminate its surroundings. To guarantee health compatibility all materials need to comply with numerous international regulations. The formulation of this outstanding compound was accordingly defined respecting almost all food contact and drinking water regulations worldwide. All used substances are listed in European and US food regulations. Features: - Good mechanical properties within the wide temperature range of -20 up to +200°C
- Complies with almost all food contact and drinking water regulations worldwide
- For static and dynamic applications
- Crosslinking agent: peroxide
Benefits:- Black FKM compound that complies with PAH Category 1
- Good mechanical properties
- Broad chemical resistance
- High purity
Notes: Ultra pure FKM with good mechanical and chemical properties for food and drinking water applicationsApprovals: - 3-A Sanitary Standard Number 18-03 Class I
- ADI free
- BAM approved maximum temperature 150 °C, maximum oxygen pressure 30 bar
- BfR XXI (Natural and synthetic rubber) Category 4
- Dlgs. 25.01.1992 n.108 Art. 2 Parte D
- D.M. 21/03/1973 (Migrations test only)
- DVGW W 270
- EC 1935/2004 article 3
- FDA - CFR 21 - 177.2600 food a) - f)
- French Arrêté 09/11/1994 (migration test)
- GB 4806.11-2016
- KIWA NSF/ANSI 51formulation
- LFGB § 30/31
- Phthalate free
- SR 817.023.21
- UBA Elastomer Guideline for cold and hot water up to 85°C
- PAH Category 1 (AfPS GS 2014:01)
- PAHs requirements acc. Regulation (EU) No 1272/2013
Information provided by Angst + Pfister |