SABIC® PP PHC27 combines very high impact resistance, also at low temperatures, with a good stiffness and
offers very good flow properties. Thanks to very low tendency to warp, it is typically used for injection moulding of crates & boxes, suitcase shells and automotive parts.
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/
medical applications.
This grade material is UL registered under File E111275 / IMDS 80775790Information provided by SABIC |