MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Lucas-Milhaupt Lithobraze 720 (BT) Silver Based Cadmium Free Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy

Material Notes:

Applications: Litho braze 720 is a good general purpose, low temperature filler metal of high fluidity for fluxless furnace brazing of stainless steels when used in dry hydrogen or inert atmospheres.

Information provided by Lucas-Milhaupt, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.67 g/cc0.349 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000339 ohm-cm
@Diameter 0.762 mm
0.00000339 ohm-cm
@Diameter 0.0300 in
annealed wire with 0.22% Li
 
Thermal PropertiesMetricEnglishComments
Melting Point 760 °C1400 °F
Solidus 760 °C1400 °FMelting Point
Liquidus 760 °C1400 °FFlow Point
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 27.2 %>= 27.2 %
Lithium, Li 0.25 - 0.50 %0.25 - 0.50 %
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 71.15 - 72.15 %71.15 - 72.15 %
 
Descriptive Properties
ColorSilver-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucas-Milhaupt Cerametil 616 Active Metal Brazing
Lucas-Milhaupt Cerametil 716 Active Metal Brazing
Indium Corp. Indalloy 215 Silver Solder Alloy
Lucas-Milhaupt Lithobraze 925 Silver Based Cadmium Free Filler Metal
Indium Corp. Indalloy 221 Silver Solder Alloy

NLUCMI41 / 18108

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.