MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow Appeel™ 55010 Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: Appeel™ 55010 is a modified polyolefin resin designed to function as a sealing layer for lidding applications, most commonly sealing to polypropylene. It is available in pellet form for use in conventional extrusion or coextrusion equipment designed to process polyethylene resins.
Uses:
  • Lidding Sealant
Applications:
  • Appeel™ 55010 has strong sealability to PP and allows a peelable seal from it
  • Boiling resistance. Appeel™ 55010 endures boiling process.
  • In the case of: OPET/adh//Appeel™ 55010, these film structures endure boiling condition at 120°C/30 min
  • Appeel™ 55010 conforms to Code #20 of the Ministry of health and Welfare Japan.

Typical structures for this lidding would be:
OPET/adhesive//Appeel 55010
PET/PE/APPELL™ 55010
Over lacquer/Print/Foil/ APPELL™ 55010
OPET/adhesive // coex film with APPELL™ 55010 This product is used as a heat seal layer in lidding material for injection molded and vacuum molded PP containers used in the packaging of puddings, jelly, and other food items.

Availability: Africa & Middle East; Asia Pacific; Latin America; Europe; North America

Agency Ratings: FDA 21 CFR 177.1520 ©3.2a

Form: Pellets

Processing Method: Blown Film; Coextrusion; Extrusion; Cast Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/ccASTM D792
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 288 °FASTM D3418
Vicat Softening Point 210 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF405 / 311098

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.