CSC4412 is a polypropylene copolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: CSC4412 has been developed especially for the automotive industry. Under body shieldings Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. Information provided by Borealis AG |