MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
EOS Titanium Ti64 DMSL on EOS M 400-4
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Titanium Alloy

Material Notes: EOS Titanium Ti64 has a chemical composition corresponding to ASTM F1472 and ASTM F2924. Ti64 is well-known light alloy, characterized by having excellent mechanical properties and corrosion resistance combined with low specific weight. Ti64 material is ideal for many high-performance applications. Parts built with EOS Titanium Ti64 powder can be machined, shot-peened and polished in as-built and heat treated states. Due to the layerwise building method, the parts have a certain anisotropy.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.41 g/ccISO 3369
Particle Size <= 63 µm<0.3 wt% above 63µm; ASTM B214
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 300 - 360
@Load 5.00 kg
EN ISO 6507-1
Tensile Strength, Ultimate 1070 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
Horizontal, Heat treated; ISO 6892-1
 1080 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
Vertical, Heat treated; ISO 6892-1
Tensile Strength, Yield 955 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
Horizontal, Heat treated; ISO 6892-1
 990 MPa
@Treatment Temp. 800 °C,
Time 7200 sec
Vertical, Heat treated; ISO 6892-1
Elongation at Break 13 %
@Treatment Temp. 800 °C,
Time 7200 sec
Horizontal, Heat treated; ISO 6892-1
 15 %
@Treatment Temp. 800 °C,
Time 7200 sec
Vertical, Heat treated; ISO 6892-1
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.5 - 6.75 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.050 %
Iron, Fe <= 0.30 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.40 %
Oxygen, O <= 0.20 %
Titanium, Ti 87.6 - 91 %Balance
Vanadium, V 3.5 - 4.5 %
Yttrium, Y <= 0.0050 %
 
Descriptive Properties
Surface roughness30-75 µmRz, after shot peening
 6-15 µmRa, after shot peening
Volume rateUp to 4 x 9,0 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NEOS956 / 280616

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.