OKULEN® 1000-Reg (PE-UHMW) Ultra high molecular weight low pressure polyethylene with regenerated (recycled) materials. Properties: conductive/Antistatic reduced; UV stabilized Color: black FN9200/similar RAL9005 Range of applications: Mechanical engineering; Conveying industry Information provided by Okulen |