MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ChenGuang SFN-1 PTFE Aqueous Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: SFN-1 is an aqueous dispersion of PTFE for general purposes with properties as below
  • With polymer solid content 60% (w/w),the mean particle size of the colloidal PTFE dispersion particles is 0.05 ~0. 5 micron.
  • With high stability against coagulation.
  • Nontoxic at room temperature.
  • Excellent chemical inertness, outstanding resistance to chemical corrosion, such as strong acid, alkali, strong oxidant, etc.
  • Outstanding resistance to heat, low temperature and abrasion.
  • Can be used at temperature range from -200°C ~ +250°C for long time.
  • Excellent electric insulation property, which is not affected by temperature and frequency.
  • Adhesive-less.
  • No absorption of water.
  • Flame-retardation, etc.
Applications:
  • Be Directly used in impregnating porous materials, such as asbestos, glass fiber, metal, ceramics and electric carbon as anti-corrosion, sealing, anti-friction and lubricating materials.
  • Be used to make protection layer by spraying or brushing on many kinds of metal or non-metal base substances, with presence of primers.
  • Be directly used for PTFE spinning.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 - 1.55 g/cc1.50 - 1.55 g/cc
Solids Content 60 %60 %
Particle Size 0.10 - 0.30 µm0.10 - 0.30 µm
pH 7.0 - 9.07.0 - 9.0
Viscosity Measure 7.0 - 10 cSt7.0 - 10 cSt
 
Thermal PropertiesMetricEnglishComments
Melting Point 317 - 337 °C603 - 639 °F
 
Descriptive Properties
ColorMilky white emulsion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU038 / 255637

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.