MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Trigonox 187-W40 Diisobutyryl peroxide
Categories: Other Engineering Material

Material Notes: Trigonox 187-W40 is an initiator (40% water-based emulsion) for (co)polymerization of vinyl chloride and vinylidene chloride. Extremely active initiator developed for the low-temperature polymerization of vinyl chloride to produce high K-value PVC.

CAS number: 3437-84-1

EINECS/ELINCS No: 222-340-0

Applications: Polymerization of vinyl chloride: Trigonox 187-W40 is a extremely active initiator especially developed for the low temperature polymerization of vinyl chloride to produce high K-value PVC. Trigonox 187-W40 can also be used in combination with other peroxides such as Di(2-ethylhexyl) peroxydicarbonate (Trigonox EHP) to increase reactor efficiency.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/cc
@Temperature 0.000 °C
Half-life 0.100
@Temperature 57.0 °C
[hr]
 1.00
@Temperature 39.0 °C
[hr]
 10.0
@Temperature 23.0 °C
[hr]
Brookfield Viscosity 200 - 1000 cP
@Temperature -10.0 °C
LVT, spindle #3
Molecular Weight 174.2 g/mol
Storage Temperature -30.0 - -25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 0.000 °C-5°C for IBC, Self-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
AppearanceWhite emulsion
Assay39.0-41.0 %
Content500 mg/kgInorganic + organic hydrolysable chloride
Content (%)9.18Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY1029 / 286552

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.