MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Swift®tak 49380 Hot Melt
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 49380 is specifically formulated for high performance laminating applications. It exhibits excellent heat resistance, moisture resistance and cold temperature resistance. 49380 has excellent specific adhesion to difficult substrates, including vinyl, paper and some plastic substrates.

Features and Benefits:

  • Good wet tack for high line speeds
  • Excellent adhesion to many substrates and stocks
  • Water resistance
  • High humidity resistance
  • High heat resistance and cold temperature resistance
  • Excellent for bonding vinyl, paper, and many plastic substrates

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 54 - 56 %
pH 4.0 - 5.5
Viscosity 2700 - 3900 cP
@Temperature 26.1 °C
Storage Temperature 65.0 - 85.0 °F
 
Descriptive Properties
ColorLight Amber
ConsistencyViscous Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL136 / 316927

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.