VISIOMER® AMA is a clear, colorless liquid with a pungent odor. Allyl methacrylate offers exceptional performance with two double bonds of different reactivity, allowing graft copolymerization in emulsions. It is used as a crosslinker, comonomer for rigid plastics, graft crosslinker and base product for the manufacture of silanes.Information provided by Evonik Operations GmbH, BL Oil Additives. |