MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Dow ENGAGE™ HM 7280 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: ENGAGE™ HM 7280 Polyolefin Elastomer resin is produced via gas phase polymerization from Dow. This is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be utilized in monolayer and coextruded films and in blends with other polyolefins to enhance melt strength and toughness of the structure.
  • High elasticity with good elastic recovery
  • High melt strength
  • Good impact strength
  • Good flow characteristics
Availability: Asia Pacific; Europe: Latin America; North America

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.886 g/cc0.0320 lb/in³ASTM D792
Mooney Viscosity 42
@Temperature 150 °C
42
@Temperature 302 °F
ML1+4; ASTM D1646
Melt Flow <= 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 0.50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Crystallinity 24.7 %24.7 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8484Compression Molded; ASTM D2240
Hardness, Shore D 2929Compression Molded; ASTM D2240
Tensile Strength at Break 5.10 MPa740 psiCompression Molded, 20 in/min; ASTM D638
 21.7 MPa
@Thickness 1.00 mm
3150 psi
@Thickness 0.0394 in
ASTM D412
Elongation at Break 310 %310 %Compression Molded, 20 in/min; ASTM D638
 640 %
@Thickness 1.00 mm
640 %
@Thickness 0.0394 in
ASTM D412
Tensile Modulus 0.00450 GPa0.653 ksi100% Secant, 20 in/min, Compression Molded; ASTM D638
Flexural Modulus 0.0253 GPa3.67 ksi1% Secant, Compression Molded; ASTM D790
 0.0282 GPa4.09 ksi2% Secant, Compression Molded; ASTM D790
Tear Strength 47.0 kN/m268 pliDie C, Compression Molded; ASTM D624
 55.0 kN/m
@Thickness 1.00 mm
314 pli
@Thickness 0.0394 in
Die C; ASTM D624
 
Thermal PropertiesMetricEnglishComments
Melting Point 116 °C241 °F
Vicat Softening Point 60.0 °C140 °FASTM D1525
Glass Transition Temp, Tg -43.0 °C-45.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF527 / 311220

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.