MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

MBA Polymers EvoSource™ 3122E Recycled PS
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: A post-consumer recycled polystyrene, suitable for injection molding and often used for extrusion applications. Available in light grey (reference 90/02), signal grey (reference 70/04) and silk grey (reference 70/44).

Information provided by MBA Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³MBA Method
Melt Flow 6.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psiISO 527-2/50
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²180/1A
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °FRange, Extrusion
 200 °C392 °FRecommended Extrusion
 190 - 230 °C374 - 446 °FRange, Injection Molding
 220 °C428 °FRecommended, Injection Molding
Mold Temperature 20.0 - 60.0 °C68.0 - 140 °FRange
 40.0 °C104 °FRecommended
Drying Temperature 70.0 °C158 °F
Dry Time 1.00 - 2.00 hour1.00 - 2.00 hour
Moisture Content 0.050 - 0.10 %0.050 - 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMBAP9805 / 282928

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.